Question

Which of the following is/are the preventions of stress-corrosion cracking?

a.

Lowering working stress below the threshold value

b.

Shot peening to produce residual compressive stresses

c.

Applying for cathodic protection

d.

Lowering working stress below the threshold value, shot peening to produce residual compressive stresses and applying for cathodic protection

Posted under Corrosion Engineering

Answer: (d).Lowering working stress below the threshold value, shot peening to produce residual compressive stresses and applying for cathodic protection

Interact with the Community - Share Your Thoughts

Uncertain About the Answer? Seek Clarification Here.

Understand the Explanation? Include it Here.

Q. Which of the following is/are the preventions of stress-corrosion cracking?

Similar Questions

Explore Relevant Multiple Choice Questions (MCQs)

Q. Corrosion fatigue is defined as the reduction of fatigue resistance due to the presence of a corrosive medium.

Q. What is meant by fatigue?

Q. What is the nature of fatigue fracture?

Q. Define the fatigue limit of a metal.

Q. Which of the following is/are the factors that influence corrosion fatigue?

Q. Which of the following is/are the facts that indicate the reduction in fatigue resistance of metal?

Q. Which of the following is/are the preventions of corrosion fatigue?

Q. Hydrogen damage refers to the mechanical damage of a metal caused by the presence of or interaction of hydrogen.

Q. Which of the following is/are the types of hydrogen damage?

Q. What is meant by hydrogen blistering?

Q. What is meant by hydrogen embrittlement?

Q. Which of the following types of hydrogen damage processes are high-temperature processes?

Q. Which of the following industries has a major concern on hydrogen blistering?

Q. Which of the following type of compounds act as an inhibitor for hydrogen-ion reduction?

Q. Which of the following metal is highly susceptible to hydrogen embrittlement?

Q. Which of the following type of corrosion in which corrosion occurs due to the presence of hydrogen sulfide?

Q. Which of the preventions is/are the preventions of hydrogen blistering?

Q. Which of the following is/are the preventions of hydrogen embrittlement?

Q. Which of the following type of corrosion is depicted in the given figure?

Q. Which of the following corrosion is depicted in the given figure?

Recommended Subjects

Are you eager to expand your knowledge beyond Corrosion Engineering? We've handpicked a range of related categories that you might find intriguing.

Click on the categories below to discover a wealth of MCQs and enrich your understanding of various subjects. Happy exploring!