Question

Which of the following common alkalies that results in stress-corrosion cracking of steel?

a.

Caustic soda

b.

Caustic soda and caustic potash

c.

Caustic potash

d.

Sodium carbonate

Posted under Corrosion Engineering

Answer: (b).Caustic soda and caustic potash

Interact with the Community - Share Your Thoughts

Uncertain About the Answer? Seek Clarification Here.

Understand the Explanation? Include it Here.

Q. Which of the following common alkalies that results in stress-corrosion cracking of steel?

Similar Questions

Explore Relevant Multiple Choice Questions (MCQs)

Q. Which of the following metal is suitable under all conditions of concentration and temperature in caustic soda?

Q. Aluminum is a very poor resistant material for handling caustic environments and rapidly attacked even by dilute solutions.

Q. Which of the following metal results in stress corrosion cracking in an ammoniacal solution?

Q. Oxygen is the primary cause of cracking in ammoniacal solution rather than nitrogen.

Q. Which of the following can be used to inhibit stress corrosion cracking in ammoniacal solutions?

Q. Which of the following is/are used for ammoniacal solution applications?

Q. Which of the following is/are the classifications of atmospheres regarding atmospheric corrosion?

Q. Which of the following is/are the primary causes of atmospheric corrosion?

Q. Corrosion of steel on the seacoast is 400 to 500 times is more corrosive than in a desert area.

Q. How many times that industrial corrosion is more corrosive than rural atmospheres?

Q. Which of the following is/are the reasons for more corrosiveness of industrial atmosphere than rural atmosphere?

Q. Which of the following alloying elements increase resistance of steel to atmospheric corrosion?

Q. Which of the following metals are widely used for atmospheric applications?

Q. Which of the following alloys is also called as weathering steels?

Q. Sheltered corrosion is the type of corrosion where moisture condenses or accumulates and does not dry out for long periods of time.

Q. Which of the following phenomenon that results in rapid corrosion on the inside of large storage tanks occurs when moisture-laden salt air is drawn in?

Q. Which of the following is/are true regarding seawater?

Q. Which of the following is/are the factors that affect corrosion in seawater?

Q. Which of the following regions of the seacoast environment shows the effect of the pitting of metals and alloys?

Q. Corrosion by seawater at greater depth is usually decreased because of the lower temperature.

Recommended Subjects

Are you eager to expand your knowledge beyond Corrosion Engineering? We've handpicked a range of related categories that you might find intriguing.

Click on the categories below to discover a wealth of MCQs and enrich your understanding of various subjects. Happy exploring!