Question

Which of the following can be used to inhibit stress corrosion cracking in ammoniacal solutions?

a.

Addition of 0.2% water

b.

Addition of 0.025% hydrazine in refrigeration

c.

Addition of oxidizing agents

d.

Either addition of 0.2% water or addition of 0.025% hydrazine in refrigeration

Posted under Corrosion Engineering

Answer: (d).Either addition of 0.2% water or addition of 0.025% hydrazine in refrigeration

Interact with the Community - Share Your Thoughts

Uncertain About the Answer? Seek Clarification Here.

Understand the Explanation? Include it Here.

Q. Which of the following can be used to inhibit stress corrosion cracking in ammoniacal solutions?

Similar Questions

Explore Relevant Multiple Choice Questions (MCQs)

Q. Which of the following is/are used for ammoniacal solution applications?

Q. Which of the following is/are the classifications of atmospheres regarding atmospheric corrosion?

Q. Which of the following is/are the primary causes of atmospheric corrosion?

Q. Corrosion of steel on the seacoast is 400 to 500 times is more corrosive than in a desert area.

Q. How many times that industrial corrosion is more corrosive than rural atmospheres?

Q. Which of the following is/are the reasons for more corrosiveness of industrial atmosphere than rural atmosphere?

Q. Which of the following alloying elements increase resistance of steel to atmospheric corrosion?

Q. Which of the following metals are widely used for atmospheric applications?

Q. Which of the following alloys is also called as weathering steels?

Q. Sheltered corrosion is the type of corrosion where moisture condenses or accumulates and does not dry out for long periods of time.

Q. Which of the following phenomenon that results in rapid corrosion on the inside of large storage tanks occurs when moisture-laden salt air is drawn in?

Q. Which of the following is/are true regarding seawater?

Q. Which of the following is/are the factors that affect corrosion in seawater?

Q. Which of the following regions of the seacoast environment shows the effect of the pitting of metals and alloys?

Q. Corrosion by seawater at greater depth is usually decreased because of the lower temperature.

Q. Which of the following impurities contaminates the brackish water due to tidal action in rivers and bays near the ocean?

Q. Which of the following metals have high resistance to crevices in quiet seawater?

Q. Which of the following alloy has high cavitation resistance that usually used for ship propellers and pumps impellers in seawater?

Q. Which of the following factors that affect the corrosivity in freshwater?

Q. Which of the following type of water is more corrosive?

Recommended Subjects

Are you eager to expand your knowledge beyond Corrosion Engineering? We've handpicked a range of related categories that you might find intriguing.

Click on the categories below to discover a wealth of MCQs and enrich your understanding of various subjects. Happy exploring!