Question

Uniform ramming of sand in green sand moulding process leads to

a.

reduced chance of gas porosity.

b.

greater dimensional stability of the casting.

c.

uniform flow of molten metal into the mould cavity.

d.

less sand expansion type of casting defect.

Answer: (b).greater dimensional stability of the casting.

Interact with the Community - Share Your Thoughts

Uncertain About the Answer? Seek Clarification Here.

Understand the Explanation? Include it Here.

Q. Uniform ramming of sand in green sand moulding process leads to

Similar Questions

Explore Relevant Multiple Choice Questions (MCQs)

Q. The yield point phenomenon observed in annealed low carbon steel is due to the presence of the following element.

Q. Wave length of X-rays is about 1 angstron, however it can not pass through a sheet of

Q. Alloying elements present in Hayness stel-lite, which has superior performance than high speed steel, are

Q. The minimum and the maximum number of members required to form a Private Limited Joint Stock Company are respectively

Q. The leaching solvent used in Baeyer's process for the purification of bauxite is

Q. Austempering process results in the formation of __________ structure.

Q. Upto the critical radius of insulation, added insulation, will

Q. Limestone is added in the blast furnace (during pig iron manufacture) to

Q. Cementite is in the lamellar form in the __________ phase of steel.

Q. To improve the machinability of steel, it is generally subjected to

Q. Silicon in steel

Q. The noble metals

Q. Which of the following is an example of cathodic protection of metals against corrosion ?

Q. Thermal efficiency of an internal combustion engine is around __________ percent.

Q. Pick out the correct combination about the role of various additives used in polymers.

Q. The lightest non-inflammable gas is

Q. Electrometallurgical methods of metal extraction is normally used for those metals

Q. Lowering of recrystallisation temperature of metals can be achieved by its

Q. An example of a buffer solution is

Q. A solid aluminium ball, when quenched in a water bath maintained at 40°C, cools down from 550°C to 450°C in 20 seconds. The expected temperature of the ball after next 20 seconds may be about __________ °C.

Recommended Subjects

Are you eager to expand your knowledge beyond Basic Chemical Engineering? We've handpicked a range of related categories that you might find intriguing.

Click on the categories below to discover a wealth of MCQs and enrich your understanding of various subjects. Happy exploring!